Special storage battery in storage process, will produce or less self discharge . The normal battery, every 1 days, the power capacity about 1% to 2% , namely a sufficient hebeike battery, storage for 1 , the power capacity of half of the loss.
A reason for the discharge
1. battery external or short circuit. When ground wire and the battery leads, or battery wrench, wire conductor will positive and negative pole , will produce severe self , will soon put the . In addition, when the of the battery shell the top cover is with an electrolyte leakage, positive and negative pole can be connected and . The
2. Storage electrode separator perforation, damage, or positive negative plates under too sediment, then the positive negative plates directly connected a short circuit, causing internal battery self discharge.
3. Impure electrolyte, containing , or add not pure , then the impurities in electrolyte with the electrolyte attached to the plates, a potential difference between impurities, will be formed the internal battery from battery into many tiny , the battery often in short-circuit state. The results that if the electrolyte 1% iron, the battery be fully discharged within 24 hours after the electricity fully discharged. The
4. Battery plate itself pure, containing more impurities, form many small battery discharge. 5. The battery a long time, water sulfuric acid in the , because the proportion of layers, the density of electrolyte on the small, formation potential difference and discharge. The
Two and the preventive
- FIAMM ASIA PACIFIC
- 21 Toh Guan Road East,
- #09-08 Toh Guan Centre,
- 608609 SINGAPORE
- Tel: +65 6867 6155
- Fax: +65 68626558
- Email: [email protected]
Industry new Your position: Home > Industry new